Experimental Study on Interfacial Bonding and Pavement Performance of Desert Sand-Fly Ash Coarse Aggregate AC-13 Asphalt Mixture
Author:
Affiliation:

1.College of Water Conservancy Architectural Engineering,Shihezi University;2.State Key Laboratory of Silicate Materials for Architectures,Wuhan University of Technology

Fund Project:

  • 摘要
  • |
  • 图/表
  • |
  • 访问统计
  • |
  • 参考文献
  • |
  • 相似文献
  • |
  • 引证文献
  • |
  • 资源附件
  • |
  • 文章评论
    摘要:

    为缓解沙漠地区道路工程中天然碎石短缺的问题,本研究以沙漠砂和粉煤灰为主要原料,通过冷粘结工艺制备了轻质多孔人工粗集料,并采用沸水试验、接触角测试、表面自由能分析、X射线衍射、扫描电镜及压汞法等方法,研究了其沥青-集料界面粘结机制及AC-13沥青混合料路用性能。结果表明:以压碎值为指标优化的配比为沙漠砂:粉煤灰:电石渣:石膏:芒硝=30:60:10:3:5,压碎值为24.5%,集料显示出轻质多孔的结构特征;沸水试验、接触角测试及表面自由能分析显示其粘附功由86.54 mJ/m2增加至92.32 mJ/m2,增幅为6.68%,沥青-集料粘结性能提升;X射线衍射、扫描电镜及压汞法结果表明该集料内部由石英微集料与钙铝硅酸盐等水化胶凝相交织构成,表面粗糙且广泛分布细小开口毛细孔;与天然集料沥青混合料相比,人工粗集料使AC-13沥青混合料最佳油石比和矿料间隙率均有一定程度的增大;动稳定度下降120 次/mm,但其马歇尔残留稳定度、冻融劈裂强度比以及低温半圆弯曲峰值荷载分别提高4.83%、4.77%和0.18 kN。可见,该粗集料通过弱碱化学吸附、多孔机械锚固与胶凝相界面连续性协同增强界面粘结,提升了沥青混合料水稳定性和低温抗裂性,可为沙漠地区道路建设提供资源化利用新途径。

    Abstract:

    In desert regions, road engineering projects are often restricted by a shortage of natural aggregate. To alleviate this problem, desert sand and fly ash were used as the primary raw materials. A lightweight porous artificial coarse aggregate was prepared via a cold bonding process. The asphalt-aggregate interfacial bonding mechanism and the pavement performance of AC-13 asphalt mixture were investigated. Boiling water tests, contact angle measurements, surface free energy analysis, X-ray diffraction (XRD), scanning electron microscopy (SEM), and mercury intrusion porosimetry (MIP) were employed. The optimized mix proportion is determined based on the crushing value. The ratio of desert sand, fly ash, carbide slag, gypsum, and mirabilite is 30:60:10:3:5. The crushing value is 24.5%. The aggregate is characterized by a lightweight and porous structure. According to boiling water tests, contact angle measurements, and surface free energy analysis, an increase in the work of adhesion from 86.54 mJ/m² to 92.32 mJ/m² is observed. This represents a 6.68% improvement. The asphalt-aggregate bonding performance is enhanced. According to XRD, SEM, and MIP results, quartz micro-aggregates and calcium-aluminum-silicate hydration gel phases are interwoven internally. Rough surfaces and widely distributed fine open capillary pores are observed. Compared with natural aggregates, both the optimum bitumen content and voids in mineral aggregate (VMA) of the AC-13 asphalt mixture are increased when the artificial coarse aggregate is used. A decrease of 120 times/mm is observed in dynamic stability. However, the Marshall residual stability, freeze-thaw splitting strength ratio, and low-temperature semi-circular bending peak load are increased by 4.83%, 4.77%, and 0.18 kN, respectively. The interfacial bonding is synergistically enhanced by weak alkaline chemical adsorption, porous mechanical anchoring, and gel phase interface continuity. Water stability and low-temperature crack resistance are improved. A new resource utilization pathway is provided for road construction in desert regions.

    参考文献
    相似文献
    引证文献
引用本文

朱建行,王勇,刘刚. 沙漠砂-粉煤灰粗集料AC-13沥青混合料界面粘结与路用性能实验[J]. 科学技术与工程, , ():

复制
分享
相关视频

文章指标
  • 点击次数:
  • 下载次数:
  • HTML阅读次数:
  • 引用次数:
历史
  • 收稿日期:2026-06-07
  • 最后修改日期:2026-10-07
  • 录用日期:2026-10-26
  • 在线发布日期:
  • 出版日期:
×
关于《科学技术与工程》全新官方网站正式上线的通知公告
关于抵制伪造参考文献学术不端行为的声明
关于规范使用生成式人工智能的声明
亟待确认版面费归属稿件,敬请作者关注